Fine grain phosphate investment; requires 15 minute benchset before placing molds into hot oven for rapid burnout; produces castings using ringless or metal ring technique; working time: 7-9 minutes; setting expansion: 1 pct; thermal expansion: 1 pct; compressive strength, wet: 500 psi; 1 liter bottle
An item used in the casting of gold alloy inlay restorations with either the thermal or hygroscopic expansion techniques during prosthetic laboratory procedures.
Classification: Other instruments and appliances, used in dental sciences; and parts and accessories, except dental drill engines, nesoi