Heat treat: (for 1085 or 1095 steel) heat at 1450 to 1500 degrees f; (for 1650 steel) heat at 1550 to 1600 degrees f; oil quench; temper 1 hour; locking feature included in head; rockwell min 73.0 to rockwell max 76.0 hardness.