Nsn used to purchase a of 16containrs to a of 39 containrs; certification pwa 1302; rc 40-45 hardness; 5000 psi strength; best finished by wet sanding; cast, crushed tungsten carbide/12% cobalt composite powder.Coatings are hard, dense and resistant to fretting type wear.Be restricted to below 1000 degrees (f)
A metallic powder used for coating metallic or nonmetallic surfaces by the welding process, to produce a surface resistant to abrasion and/or corrosion. It may be applied with an oxy-acetylene torch, furnace, or with a spray weld gun.
Classification: Welding machine parts and parts of apparatus